Blast-resistant glazing: explained and simplified
In most explosive incidents the greatest cause of injury is not the blast itself — it is flying glass. Blast-resistant glazing does not stop a blast.
In most explosive incidents the greatest cause of injury is not the blast itself — it is flying glass. Blast-resistant glazing does not stop a blast. It controls where the glass goes. Getting that right depends on describing the load properly, and on understanding that the glass is only one part of what has to survive.
What actually arrives at the window
An explosion sends out a shock front. Ahead of it the air is undisturbed; behind it the pressure jumps almost instantly to a peak, then decays back to ambient. It then falls below ambient before recovering. That second part matters, and it is routinely ignored.
- The positive phase pushes the glazing inwards. It is short, sharp and carries most of the energy.
- The negative phase follows, as air rushes back to fill the partial vacuum at the seat of the explosion. It is weaker but lasts longer, and it pulls the glazing outwards.
Rebound during the negative phase is a genuine failure mode, not a footnote. In published trial records, glazing has been drawn out of its opening on the way back after surviving the way in. Anchorage and fixings have to work in both directions.
Incident or reflected — ask this first
This is the most common and most expensive misunderstanding in facade blast work, and it is worth settling before any other conversation.
If a specification states a pressure without saying whether it is incident or reflected, the difference between the two readings is at least a factor of two on the design load. We ask, every time. Where it cannot be established we take the stated figure as incident and apply a reflection factor, and we say so on the face of the calculation.
The three numbers
The three are related. Idealising the decay as a straight line — the standard simplification for design — gives ir ≈ ½ × Pr × td. So any two of the three define the third. That is why a specification giving pressure and duration is complete, and one giving pressure alone is not, unless the duration can be inferred.
Which number governs, and why
A window is not a static object. It has mass and stiffness, so it has a natural period — the time it takes to complete one cycle of vibration. For architectural glazing that period is typically in the range of roughly ten to thirty milliseconds, depending on size, thickness and support.
What governs the design is the ratio of the load duration to that natural period. Blast engineers describe three regimes, and they are usually drawn on a pressure–impulse diagram.
As a rule of thumb, a load lasting less than about a third of the natural period behaves impulsively, and one lasting more than about three times the natural period behaves quasi-statically. Between those, both parameters matter.
Why a process specification can give one number
A vapour cloud explosion is a large volume of gas burning relatively slowly. Its positive phase runs to tens or hundreds of milliseconds — far longer than a window's natural period. The response is quasi-static, and peak pressure is the governing parameter.
A high-explosive detonation is the opposite. The positive phase may be only a few milliseconds. The response is impulsive, and two events with the same peak pressure and different durations produce entirely different outcomes.
This is why a process facility specification stating a peak pressure and nothing else is usually workable, while a security specification stating a peak pressure and nothing else is not. The first implies a long-duration deflagration. The second implies a detonation, where the duration could be two milliseconds or twenty — and those demand entirely different glazing.
Where only a peak pressure is given and the source is not obvious, we ask for the positive phase duration. If it cannot be obtained we adopt a conservative assumption, state it plainly on the calculation, and flag it for the project engineer to confirm. We do not quietly invent the missing figure.
The units
The same load appears in different units depending on where the specification was written, not on which industry it belongs to. Process and security work both use both systems, and it is common to see them mixed within a single project.
Where the numbers come from
- For defence and government work, the applicable antiterrorism design criteria, which set the required level of protection If none of these is available, a charge weight, its TNT equivalent and the standoff distance is enough — pressure, duration and impulse can all be derived using the established scaled-distance relationships, provided the detonation geometry is also stated. A surface burst at grade produces a substantially higher load than the same charge in free air.
Confirm the standoff distance available on site before anything else. Blast pressure falls away rapidly with distance, so standoff is by a wide margin the cheapest protection available — and once the site layout allows it, it costs nothing.
How much glass is acceptable — hazard ratings
The second half of a blast specification is the outcome you will accept. The American system measures it directly: a witness panel is set three metres behind the opening, and the rating records how far the glass travelled.
Conditions 1 and 2 are the usual target for occupied buildings. The step from Condition 4 to Condition 5 is the difference between glass on the floor and glass at the height of a person standing at a desk.
The classification systems
The EN classes make the point of Section 3 explicit: they are defined by pressure and impulse together, over a positive phase of at least 20 milliseconds. ER1 covers 50 to 100 kPa with 370 to 900 Pa·s; ER2 covers 100 to 150 kPa with 900 to 1,500 Pa·s. A load meeting the pressure band but not the impulse band does not fall in the class.
An EN 13541 ER2 classification does not carry a GSA Performance Condition, and a GSA Condition 2 does not carry an EN class. Where a project cites both, each has to be evidenced separately.
The glass alone is never the rating
A blast rating belongs to a complete assembly — the glass, the frame, the bite and gaskets, the beads or pressure plate, the hardware, and the anchorage into the structure. The load has to travel all the way from the glass surface into the building frame, and it will find the weakest link on the way.
- The weak link is rarely the glass. In published blast trials the failures are overwhelmingly failures of fixings, bolts, screws and adhesive bonds.
- Everything must work in reverse too. The negative phase reverses the reaction at every fixing. A detail that only bears in compression is not adequate.
- The reactions have to go somewhere. Every blast-rated element delivers a load into the surrounding structure. That structure must be verified to receive it — which is why we state the anchorage reactions in every submittal.
- Glass edge cover and bite are part of the design. Too little bite and the pane pulls out of the rebate before the glass has done any work at all.
New build or retrofit
Film on its own, with no edge-retention anchoring, holds the broken glass together but does not hold it in the opening. The anchoring is what turns film into a blast system.
The range at British Aluminium
We supply the complete range across both certification systems — EN and US — as certified assemblies, not assembled from separately rated parts.
Aluminium and steel framed glazing, doors and public counters EN 1522 / EN 1063 · UL 752 / NIJ 0108.01 Acoustic systems 80 mm and 100 mm double-glazed partitions, acoustic doors and screens EN ISO 10140 / EN ISO 717-1 · ASTM E90 / E413 / E1332 Combined performance Fire with blast, ballistic with acoustic, and other multi-requirement assemblies Certified per configuration The easiest way to start: send us the blast design basis — or the peak pressure, whether it is incident or reflected, and the charge weight and standoff if you have them — with the elevation and window schedule. We will confirm the load in both metric and imperial, tell you whether the duration needs to be established, and identify which of our systems meets it.
Issued for information. Selection of the design threat, the blast load and the required hazard rating is the responsibility of the project's security consultant, blast engineer and the authority having jurisdiction. This document does not constitute blast engineering advice. Standards are cited as at the date shown and this guide is revised without notice; always work from the current issue.
The full guide
This page gives the text of our technical guide. The tables, charts and quick-reference sheet are in the PDF: download the full guide.
Related
Have a project requirement?
Send your drawings, specification and project location. Tell us what the opening needs to achieve and where you need support.